flaring stainless steel lines
I had to shorten a stainless brake line and can't get get the end reflared. Problem is the line does'nt stay clamped in the tool no matter how hard I try to clamp it, it slides thru. The (double) flaring tool is brand new. If I heat the brakeline prior to flaring, will this mess with the stainless hardness? Any tips ?