My 70 Dart
I am very frustrated right about now. I have access to a MIG, but I keep burning through. I'm practicing on some 18 ga steel that I picked up. I can't see, I have to use one hand to hold the shield and weld at the same time. It's a real PITA just to practice when you can't even see! So that method is not working out at the moment. Next on to the lead, body solder. I was able to get some, but I forgot the flux. It seems all you can get is lead free stuff. AKA called tinning flux? I hope thats the reason why that method is not working for me either. It seems as soon as I get the lead even close to melting, it just runs away. There has to be an easier way than these two. I had to walk away from this for now. Calm down and try again later today, most likely tomorrow.