Pro Touring 10K

Moving on to the deck lid. This is the one area that has a little rust. The rest of the is rust free so I won't complain to much. For what ever reason the left side is by far the worst. Dealing with multiple layers of panels makes for a little more work as well. first the lip that folds over to the outer skin needs to come off. Then the damaged area under the first layer can be cut out. then you will need to make a new filler panel.al little more trimming and I can start to weld every thing in place. A couple of more evenings and it will be ready for filler work. then in the booth to epoxy prime.