Cinnamon 75 Duster \

I was sealing joints in floor at work with this stuff and got this idea. Tested the flow on some plastic and liked the way it stuck to it. I rigged a poly tube and a piece of a busted tube from a telescoping magnet.to get through the grate. Ran it in against the front and let it flow down over the joint where the metal layers together. Cleaned up the mess on the grid with mineral spirits. Then I blew it back uphill with compressed air to force more toward the joint. Made one big oops in not blowing out the cowl first. Hemlock needles had gotten in there since I cleaned it and some churned up and got in the goo.

2016-03-30 05_41_27.jpg

2016-03-30 05_40_43.jpg