1970 Duster project in Sweden

Very nice metal work Trebor75. Btw here in the states we use a different pinhole filler now than the red scratch and pinhole filler putty that used to be prevalent years ago.

In more common use now is a 2 part fine polyester pinhole filler called Evercoat that is used over the the top of the body filler. Being that these are both polyester based they bond together nicely.

The older red scratch putty "red lead" or "nitrostan" has a tendency to crack over time as it ages and shrinks.
Thanks! I'm a beginner when it comes to body work. It took quite some time to get it somewhat straight. I hope it will come out decent enough. It's funny that you mention the putty filler. I was visiting a friend in CA and I bought some different brands of putty. We dont have that stuff over here. And that red one in the picture that you mention was a disappointment. I actually sanded it all down and used only PP100. Today I found that I also purchased a way better glazing putty on my visit too. So on the other repairs I make I will probably use that as a final layer before priming. Thanks for explaing!