1969 dart rebuild !

Thanks! Yes, they are 3/8 thick so we got the cut offs and did some test runs for the heat range, once happy with how the weld penetration was, it was tacked then the ends were welded, heated the center up, tacked, welded then the ends got a second weld cause the chamfer was deep and wide. I’m pretty pleased with how it turned out.