Faceplated 833 4 Speed

So the carbide insert didn't care about the interrupted cut? At least until all the teeth were gone? Usually carbide hates an interrupted cut.

What wire did you use? I don't have a wire feed here so I'll just TIG it.

Maybe I should just face plate it if Liberty will sell the plates.

Carbide might have cared a little, but did the job :) I used ER70S-6 filler, quite a bit softer than the parent metals. I think the faceplate parts are case hardened 9310.

Grant