67/68/69 cuda dilemma

Starting fab on the inner trunk lip section. Theres more perforation on the outer skin lip once we opened it up. I think I am going to naval jelly this area and see how bad it is. May be worthy of just tack welding the holes up and applying a generous amount of epoxy primer over the clean pitted metal and leaving it alone.

20241110_134600.jpg

20241110_141900.jpg

20241110_141904.jpg

20241110_143506.jpg

20241110_143531.jpg

20241110_144844.jpg