Stop in for a cup of coffee

Anybody worked with this stuff before? I've had good results from other VHT products

VHT High temp Black Wrinkle Aerosol SP201
Let talk instructions..
Prep is everything
Fallow there instructions to the T.(letter)
Cross hatching spray is a must.
After first coat , I wait 7 minutes then hit it good with out runs.
I like 4 coats myself, then Be Very Carful not to get the surface to hot, when you see smoke back up your heat gun, keep the heat going but remember that if you have a small part to never keep the heat on it so to not over cook it, I think 230 is where you want to keep it till you see the wrinkles show up.
Been preparing these, I will be painting today if nothing gets in my way

20250319_175306.jpg

20250319_175344.jpg

20250319_175356.jpg